Catherine Lucero, Robert Spragg, Dale P. Bentz, Daniel S. Hussey, David L. Jacobson, Jason Weiss
… prepared with water to cement ratios, (w/c), of 0.36, 0.42 and 0.50 by mass. The mortar specimens were conditioned to … by 38 %, 20 %, and 26 % in mortars with a w/c of 0.36, 0.42 and 0.50, respectively. At high CaCl2 concentrations (29.8 …