Stress corrosion behavior of X7050-T76351 alloy aluminum plate:

Published

Author(s)

B T Sanderson, W F Gerhold
Citation
- NBS IR 76-1166
Report Number
NBS IR 76-1166

Citation

Sanderson, B. and Gerhold, W. (1976), Stress corrosion behavior of X7050-T76351 alloy aluminum plate:, , National Institute of Standards and Technology, Gaithersburg, MD, [online], https://doi.org/10.6028/NBS.IR.76-1166 (Accessed November 14, 2026)