Stress corrosion behavior of high strength corrosion resistant materials ::progress report

Published

Author(s)

W F Gerhold
Citation
- NBS report ; 9990
Report Number
NBS report ; 9990

Citation

Gerhold, W. (1969), Stress corrosion behavior of high strength corrosion resistant materials ::progress report, , National Institute of Standards and Technology, Gaithersburg, MD, [online], https://doi.org/10.6028/NBS.RPT.9990 (Accessed November 18, 2026)
Additional citation formats

Issues

If you have any questions about this publication or are having problems accessing it, please contact [email protected].

Created January 1, 1969, Updated May 19, 2023