Kruger, J.
, Ambrose, J.
and Kodama, T.
(1975),
The role of passive film growth kinetics and properties in stress corrosion and crevice corrosion susceptibility:, , National Institute of Standards and Technology, Gaithersburg, MD, [online], https://doi.org/10.6028/NBS.IR.75-916 (Accessed November 14, 2026)