Skip to main content
U.S. flag

An official website of the United States government

Official websites use .gov
A .gov website belongs to an official government organization in the United States.

Secure .gov websites use HTTPS
A lock ( ) or https:// means you’ve safely connected to the .gov website. Share sensitive information only on official, secure websites.

Nanoindentation Behavior and Mechanical Properties Measurement of Polymeric Materials

Published

Author(s)

Robert F. Cook, Michelle Oyen
Citation
International Journal of Materials Research
Volume
98
Issue
5

Citation

Cook, R. and Oyen, M. (2007), Nanoindentation Behavior and Mechanical Properties Measurement of Polymeric Materials, International Journal of Materials Research, [online], https://tsapps.nist.gov/publication/get_pdf.cfm?pub_id=854351 (Accessed November 13, 2026)
Additional citation formats

Issues

If you have any questions about this publication or are having problems accessing it, please contact [email protected].

Created May 1, 2007, Updated February 19, 2017