Cook, L.
and Bonnell, D.
(1987),
Model for molten salt corrosion of (Co, Cr)-based superalloys:, , National Institute of Standards and Technology, Gaithersburg, MD, [online], https://doi.org/10.6028/NBS.IR.87-3628 (Accessed October 24, 2026)