Kruger, J.
, Ugiansky, G.
and Ambrose, J.
(1968),
Investigation of the directional effects in the stress corrosion of aluminum alloys ::final report, , National Institute of Standards and Technology, Gaithersburg, MD, [online], https://doi.org/10.6028/NBS.RPT.9821 (Accessed November 16, 2026)