Atom-Probe Tomographic Study of ¿/¿' Interfaces and Compositions in an Aged Co-Al-W Superalloy

Published

Author(s)

Eric Lass, Kil-Won Moon, Maureen E. Williams, Carelyn E. Campbell, Ursula R. Kattner, David C. Dunand, Peter J. Bocchini, David N. Seidman

Abstract

Atom-probe tomography (APT) is utilized to investigate, in a Co-9.7Al-10.8W at.% alloy aged at 900 °C for 1000 h, the phase composition and partitioning behavior of the two-phase ɣ(f.c.c.)/ɣ'(L12) microstructure. The APT composition of the ɣ-matrix (Co-8.97Al-5.69W at.%) agrees well with a previously reported measurement made by energy-dispersive X-ray spectroscopy; however, the composition of the ɣ'(L12) precipitates (Co-10.03Al-12.48W at.%) is slightly richer in W and Al, and leaner in Co. Partitioning coefficients and Al interfacial excess have also been calculated.
Citation
Scripta Materialia
Volume
68

Keywords

¿/¿' Co-based superalloys, Atom-probe tomography, Co-Al-W

Citation

Lass, E. , Moon, K. , Williams, M. , Campbell, C. , Kattner, U. , Dunand, D. , Bocchini, P. and Seidman, D. (2012), Atom-Probe Tomographic Study of ¿/¿' Interfaces and Compositions in an Aged Co-Al-W Superalloy, Scripta Materialia, [online], https://doi.org/10.1016/j.scriptamat.2012.11.035 (Accessed September 10, 2026)
Additional citation formats

Issues

If you have any questions about this publication or are having problems accessing it, please contact [email protected].

Created December 11, 2012, Updated October 12, 2021
Was this page helpful?