March 15, 1999
Author(s)
S P. Alpay, V Nagarajan, Leonid A. Bendersky, Mark D. Vaudin, S Aggarwal, R Ramesh, Alexander L. Roytburd
PbZr 0.2Ti 0.8O 3(PZT) thin films with and without La 0.5Sr 0.5CoO 3(LSCO) electrodes were grown epitaxially on (001) SrTiO 3 (STO) at 650 C by pulsed laser deposition. The domain structure of the 400 nm thick PZT films with different electrode layer